Mechanical Properties Metric English Comments
Fatigue Strength 55.0 MPa

@# of Cycles 100000
7980 psi

@# of Cycles 100000
BASF Ultrason S 2010 G6 30% Glass Filled PSU
Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Fatigue Strength 55.0 MPa

@# of Cycles 10000
7980 psi

@# of Cycles 10000
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..