Polymer Property : Fatigue Strength = 79800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fatigue Strength <= 550 MPa

@# of Cycles 100000
<= 79800 psi

@# of Cycles 100000
ArcelorMittal FB 590 Hot rolled ferrite-bainite steel
Available in the following: uncoated (HDT590F)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It comprises four strength levels: ..
Copyright © lookpolymers.com All Rights Reserved