Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 560 MPa @# of Cycles 1.00e+7 |
81200 psi @# of Cycles 1.00e+7 |
unnotched, stress range 0 to 560 Mpa |
TIMET TIMETAL® 834 (Ti-5.8Al-4Sn-3.5Zr-0.7Nb-0.5Mo-0.35Si-0.06C) Titanium Alloy High-Strength, High Temperature, Creep Resistant AlloyIndustry Specifications: France: T-A6EZ r4Nb.Features: TIMETAL 834 is a near alpha titanium alloy offering increased tensile strength and creep.. |
|||
Fatigue Strength | <= 560 MPa @# of Cycles 2.00e+6 |
<= 81200 psi @# of Cycles 2.00e+6 |
|
ArcelorMittal Complex Phase Steel 800 Y500 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT780C) and electrogalvanized (HCT780C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |
|||
Fatigue Strength | <= 560 MPa @# of Cycles 1.00e+7 |
<= 81200 psi @# of Cycles 1.00e+7 |
|
ArcelorMittal Complex Phase Steel 800 Y500 Very high strength steel, Cold Rolled Steel Available in the following: uncoated (HCT780C) and electrogalvanized (HCT780C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r.. |