Charpy Impact 13.56 J
10.00 ft-lb
Crucible Steel CPM® S30V® Stainless Steel
CPM S30V is a martensitic stainless steel designed to offer the best combination of toughness, wear resistance and corrosion resistance. Its chemistry has been specially balanced to promote the form..