Mechanical Properties Metric English Comments
Charpy Impact 12.0 J
8.85 ft-lb
after 8000 hours at 870°C
Haynes 188 alloy, plate at RT after 1000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Charpy Impact 12.0 J
8.85 ft-lb
after 8000 hours at 870°C
Haynes 188 alloy, plate at RT after 16000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Charpy Impact 12.0 J
8.85 ft-lb
after 8000 hours at 870°C
Haynes 188 alloy, plate at RT after 4000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Charpy Impact 12.0 J
8.85 ft-lb
after 8000 hours at 870°C
Haynes 188 alloy, plate at RT after 8000 hours at 870°C (1600°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Charpy Impact 12.0 J
8.85 ft-lb
Typical (Longitudinal)
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability
Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c..
Charpy Impact 12.0 J
8.85 ft-lb
Austenitizing Temperature- 1120°C
Crucible Steel CPM® 15V® Tool Steel
CPM 15V is intended for applications requiring exceptional wear resistance. It has more vanadium carbides in its microstructure than CPM 10V and provides more wear resistance and longer tool life in..
Charpy Impact 12.0 J
8.85 ft-lb
tempering at 300°C (570°F). Hardened at 960°C (1760°F). Quenched in air. Tempered twice.
Assab Steels CALMAX Plastic Mold Material
CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo..
Charpy Impact 12.0 J

@Diameter 25.0 mm
8.85 ft-lb

@Diameter 0.984 in
bar
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..