Mechanical Properties Metric English Comments
Charpy Impact 10.8 - 16.3 J
8.00 - 12.0 ft-lb
Austenitizing temp 1725°F, Tempering temp 400-1000°F
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh..
Charpy Impact 13.6 - 16.3 J
10.0 - 12.0 ft-lb
Notched; 44 HRC
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel
Description: Thermodur® 2343 is a single melt Extra Fine Structure (EFS) hot work die steel and Supplied in the annealed conditionCharacteristics: Good toughness; Moderate high-temperature strength..