Mechanical Properties Metric English Comments
Charpy Impact >= 180 J
>= 133 ft-lb
Industeel CLC 18.10 LN Nitrogen Containing 18Cr-10Ni Austenitic Stainless Steel
Description: CLC 18.10LN is a 18Cr-10Ni austenitic stainless steel with specific Nitrogen additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior ..
Charpy Impact 180 J

@Temperature -20.0 °C
133 ft-lb

@Temperature -4.00 °F
Longitudinal
Bisalloy Steels BisPlate 70 Thickness >80-100 mm
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat..
Charpy Impact >= 180 J
>= 133 ft-lb
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel
Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k..
Charpy Impact 180 J

@Temperature -20.0 °C
133 ft-lb

@Temperature -4.00 °F
Longitudinal
Bisalloy Steels BisPlate 70 Thickness 16-80 mm
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat..
Charpy Impact 180 J

@Temperature -20.0 °C
133 ft-lb

@Temperature -4.00 °F
Longitudinal
Bisalloy Steels BisPlate 70 Thickness 5 -
Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat..
Copyright © lookpolymers.com All Rights Reserved