Mechanical Properties Metric English Comments
Charpy Impact 217 J

@Temperature 23.0 °C
160 ft-lb

@Temperature 73.4 °F
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Charpy Impact 217 J
160 ft-lb
V-Notch
Crucible Steel XM-19 Stainless Steel
Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio..