Charpy Impact 220 J

@Temperature -196 °C
162 ft-lb

@Temperature -321 °F
Typical
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel
Description: CLC 18-9L is a 18Cr-9Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This k..