Polymer Property : Charpy Impact = 21.69 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 21.69 J
16.00 ft-lb
U-Notch
Latrobe Lescalloy® 35NCD16 VAC-ARC High Strength Alloy Steel
LESCALLOY 35NCD16 VAC-ARC is a high strength, low alloy vacuum arc remelted steel which takes its name from the French industry designation. The combination of high strength, high fracture toughnes..