Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 122 - 224 J | 90.0 - 165 ft-lb | V-notch |
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |