Charpy Impact 32.0 J
23.6 ft-lb
tempering at 600°C (1110°F). Hardened at 960°C (1760°F). Quenched in air. Tempered twice.
Assab Steels CALMAX Plastic Mold Material
CALMAX is a chromium-molybdenum-vanadium alloyed steel characterized by:High toughnessGood wear resistanceGood through hardening propertiesGood dimensional stability in hardeningGood polishabilityGo..