Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact = 24.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 24.0 J
17.7 ft-lb
Haynes 230® alloy, plate, 1000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Charpy Impact 24.0 J
17.7 ft-lb
aged 4000 hours at 760°C (1400°F)
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Charpy Impact 24.0 J
17.7 ft-lb
Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C
Crucible Steel Nu-Die® V (AISI H13) Hot Work Tool Steel
Nu-Die® V (AISI H13) has been the most popular, and perhaps the most versatile hot work tool steel available for many years. It provides a good balance of toughness, heat check resistance and tempe..
Charpy Impact 24.0 J
17.7 ft-lb
Austenitizing Temperature- 1010°C, air cool, Tempering Temperature- 605°C
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel
Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b..
Charpy Impact 24.0 J
17.7 ft-lb
Haynes 230® alloy, plate, 1000 hours exposure at 760°C (1400°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..
Charpy Impact 24.0 J
17.7 ft-lb
Latrobe Staminal™ Shock Resisting Die Steel
Staminal is an air or oil hardening die steel containing a large percentage of nickel combined with a proper balance of other alloying elements for deep hardening and extreme toughness. For tools, ..