Polymer Property : Charpy Impact = 25.8 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 25.8 J
19.0 ft-lb
V-Notch
International Mold Steel Premium H13 Hot Work Die and Mold Steel
Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti..