Polymer Property : Charpy Impact = 250 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 339 J

@Temperature -73.0 °C
250 ft-lb

@Temperature -99.4 °F
Typical V-Notch
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work
Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r..