Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 351 J @Temperature -196 °C |
259 ft-lb @Temperature -321 °F |
heat treated at 1121°C (2050°F) then rapid quenched |
Haynes Hastelloy® C-22® alloy, 0.71-3.2 mm thick sheet, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Charpy Impact | 351 J @Temperature -196 °C |
259 ft-lb @Temperature -321 °F |
heat treated at 1121°C (2050°F) then rapid quenched |
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Charpy Impact | 351 J @Temperature -196 °C |
259 ft-lb @Temperature -321 °F |
heat treated at 1121°C (2050°F) then rapid quenched |
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |