Mechanical Properties Metric English Comments
Charpy Impact 27.1 J
20.0 ft-lb
V-Notch; Air Cooled from 1010°C; 650°C Temper Temperature
Latrobe LSSâ„¢ H11 Hot Work Tool Steel (ASTM H11)
TLS H11 hot work tool steel is a 5% chromium hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool steel. This provides..
Charpy Impact 27.1 J

@Temperature 23.0 °C
20.0 ft-lb

@Temperature 73.4 °F
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for..
Charpy Impact 27.1 J
20.0 ft-lb
Solution treated plus 982°C for 500 hours
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening..
Charpy Impact 27.1 J
20.0 ft-lb
notched
Carpenter AerMet® 310
AerMet 310 alloy possesses higher hardness and strength than AerMet 100 alloy while maintaining exceptional ductility and toughness. At a 310 ksi (2137 MPa) ultimate tensile strength, AerMet 310 all..