Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 312 J | 230 ft-lb | Typical |
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |