Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 54.0 J | 39.8 ft-lb | V-notch |
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Charpy Impact | 54.0 J | 39.8 ft-lb | V-notch |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Charpy Impact | 54.0 J @Temperature -17.8 °C |
39.8 ft-lb @Temperature 0.000 °F |
V-notch |
Latrobe Lescalloy® HY-180 VIM-VAR ; 4.01 - 8.00 thickness High Strength Alloy Steel LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR vacuum induction melted followed by vacuum arc remelting) to provide superi.. |