Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 5.80 J @Temperature 22.8 °C |
4.28 ft-lb @Temperature 73.0 °F |
ISO179 |
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced TECAPEEK® ST is a multipurpose semi-crystaline material from the polyaryletherketone family based on PEKEKK that features improved mechanical properties at higher temperatures. The benefits of TECA.. |