Mechanical Properties Metric English Comments
Charpy Impact >= 70.0 J

@Temperature -50.0 °C
>= 51.6 ft-lb

@Temperature -58.0 °F
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re..
Charpy Impact >= 70.0 J

@Temperature -50.0 °C
>= 51.6 ft-lb

@Temperature -58.0 °F
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red..
Charpy Impact 70.0 J

@Temperature 250 °C
51.6 ft-lb

@Temperature 482 °F
V-notch. Short transverse direction. 47 HRC
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Charpy Impact 70.0 J

@Temperature 250 °C
51.6 ft-lb

@Temperature 482 °F
V-notch. Short transverse direction. 50 HRC
Assab Steels DIEVAR Hot Work Steel
DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i..
Charpy Impact 70.0 J
51.6 ft-lb
Typical Toughness (long)
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment)
Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g..
Copyright © lookpolymers.com All Rights Reserved