Mechanical Properties Metric English Comments
Charpy Impact 12.2 J
9.00 ft-lb
As Cast
Weartech International WT-6 Cobalt Hardfacing & Wear Resistant Alloy
Applications: engine valves, pump shafts & sleeves, hot cutting & rotary knives, high pressure high temperature valves, extrusion screwsInformation provided by Weartech International
Charpy Impact 12.2 J

@Temperature 20.0 °C
9.00 ft-lb

@Temperature 68.0 °F
Average CharpyV-notch from 6.3" plate at 387 HB
EDRO EDRO400™ #40 Prehardened Insert Quality Martensitic Stainless Steel
EDRO400™ is a remelted 400 series martensitic stainless steel supplied prehardened to 40 HRC (375 HB).EDRO400™ is characterized by excellent polishability, superior corrosion resistance, high leve..
Charpy Impact 12.2 J
9.00 ft-lb
V-notch
Crucible Steel CPM® Nu-Die® EZ Tool Steel
CRUCIBLE CPM Nu-Die EZ is a new, patented die and mold steel designed for service as die casting dies and plastic injection molds. It is supplied in the prehardened condition, and is easily machined..
Charpy Impact 12.2 J
9.00 ft-lb
Solution treated plus 871°C for 500 hours
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening..
Charpy Impact 12.2 J
9.00 ft-lb
Solution treated at 816°C plus 168 hours
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening..
Charpy Impact 12.2 J
9.00 ft-lb
V-Notch; Oil Quenched from 1177°C; 650°C Temper Temperature
Latrobe LSS™ H21 Hot Work Tool Steel (ASTM H21)
TLS H21 hot work tool steel is a low-carbon, tungsten hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is intended for elevated-temperature service ..
Charpy Impact 12.2 J
9.00 ft-lb
V-Notch; Oil Quenched from 1177°C; 370°C Temper Temperature
Latrobe LSS™ H21 Hot Work Tool Steel (ASTM H21)
TLS H21 hot work tool steel is a low-carbon, tungsten hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is intended for elevated-temperature service ..