Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 8.13 - 9.49 J | 6.00 - 7.00 ft-lb | RT |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |