Polymer Property : Charpy Impact = 9.50 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 12.9 J
9.50 ft-lb
V-Notch; Air Cooled from 1010°C; 490°C Temper Temperature
Latrobe LSSâ„¢ H14 Tool Steel (ASTM H14)
TLS H14 tool steel is a 5%-chromium hot work steel to which tungsten has been added for improved high-temperature properties and heat resistance. It is a deep-hardening, airhardening steel that exh..