Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.0780 GPa | 11.3 ksi | ASTM D790 |
Dow Engage® 8480 Polyolefin Elastomer Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari.. |