Mechanical Properties Metric English Comments
2% Secant Modulus 0.104 GPa
15.1 ksi
ASTM D790
Dow Engage® 8540 Polyolefin Elastomer
Description: Engage® 8540 polyolefin elastomer is an ethyleneoctene copolymer that is well suited to foamed applications and offers excellent performance for profile extrusion of tubing and hoses. ..