Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 2% Secant Modulus = 0.179 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.179 GPa
26.0 ksi
ASTM D790
Noble Polymers Ecobarrier™ 2614 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
2% Secant Modulus 0.179 GPa
26.0 ksi
ASTM D790
Noble Polymers Ecobarrier™ 2618 Thermoplastic Olefin (TPO)
Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa..
2% Secant Modulus 0.179 GPa
26.0 ksi
Crosshead Speed - 1/2 in/min; ASTM D790
LyondellBasell Petrothene® NA860008 Low Density Polyethylene
ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel..
2% Secant Modulus 0.179 GPa
26.0 ksi
Crosshead Speed - 1/2 in/min; ASTM D790
LyondellBasell Petrothene® NA860241 Low Density Polyethylene
ApplicationsPETROTHENE NA 860 is a series of medium flow, low density polyethylene resins for the injection molding of caps, closures and other specialty applications. These resins exhibit an excel..
Copyright © lookpolymers.com All Rights Reserved