2% Secant Modulus 0.414 GPa
60.0 ksi
0.5"/min; ASTM D790
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade
PETROTHENE GA574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items.Regulatory Status: GA574189 meets th..