Mechanical Properties Metric English Comments
2% Secant Modulus 0.650 GPa
94.3 ksi
500mm/min; ASTM D638
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical
2% Secant Modulus 0.650 GPa
94.3 ksi
500mm/min; ASTM D638
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical