Mechanical Properties Metric English Comments
2% Secant Modulus 0.00530 GPa
0.769 ksi
ASTM D790
Dow Engage® ENX 7458.00 Ethylene-Butene Copolymer
Description: ENX 7458.00 is a unique broader molecular weight distribution ethylene-butene copolymer that offers excellent flow and impact properties and is ideally suited for plastics modification...