Mechanical Properties Metric English Comments
2% Secant Modulus 0.0726 GPa
10.5 ksi
ASTM D790
Dow Engage® 8450 Polyolefin Elastomer
Description: Engage® 8450 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It has excellent compatibility with other p..