Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 1.044 GPa | 151.4 ksi | Crosshead speed - 0.5" min; ASTM D790 |
LyondellBasell Alathon® M5040 High Density Polyethylene ApplicationsALATHON M 5040 is a copolymer with broad molecular weight distribution. This resin exhibits excellent color, low odor, and good processing stability. Typical applications for this res.. |