Mechanical Properties Metric English Comments
2% Secant Modulus 1.23 GPa
179 ksi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® H6030 High Density Polyethylene
ApplicationsALATHON H 6030 is a homopolymer that provides enhanced processability, excellent stiffness and short molding cycles. Typical applications include thin wall and deep-drawRegulatory Statu..