Polymer Property : 2% Secant Modulus = 32.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.221 GPa
32.1 ksi
12.7mm/min; ASTM D790
Westlake EM184AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM184 is a low density injection-molding formulation suggested for the production of closures where a high melt index is needed to meet shrinkage requirements and f..