Mechanical Properties Metric English Comments
2% Secant Modulus 0.255 GPa
37.0 ksi
12.7 mm/min, Flexural; ASTM D790
Westlake EC4041AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC4041 is recommended for use in the boardstock coating industry. The resin has low neck-in and good drawdown characteristics. Coatings produced from EC4041 have ex..