Mechanical Properties Metric English Comments
2% Secant Modulus 0.0679 GPa
9.85 ksi
ASTM D790
Dow Engage® ENR 7086.01 Ethylene-Butene Copolymer
Description: ENR 7086.01 is a revolutionary new ethylene-butene copolymer with a broader molecular weight distribution and much higher levels of long chain branching than other commercially availabl..