Tangent Modulus 1050 MPa
153000 psi
ASTM D790
Noble Polymers Regis™ 155120 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..