Polymer Property : Tangent Modulus = 115000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tangent Modulus 790 MPa
115000 psi
ASTM D790
Flint Hills P5M4R-034 Polypropylene Random Copolymer
Features: Radiation resistant. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: medical devicesInformation Provided by Flint Hills Resources