Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tangent Modulus | 1590 MPa | 230000 psi | ASTM D790 |
Noble Polymers Forte™ 4CPP093 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Tangent Modulus | 1590 MPa | 230000 psi | ASTM D790 |
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |