Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tangent Modulus 1540 MPa
224000 psi
ASTM D790
Noble Polymers Regis™ 225104 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..