Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tangent Modulus 1650 MPa
239000 psi
ASTM D790
Flint Hills H0500HN Polypropylene Homopolymer
Features: Nucleated and long term heat aging (LTHA). Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: medical partsInformation Provided by Flint ..