Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.0621 MPa
9.00 psi
ASTM D624
Arlon 55149R062 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass
Adhesive Bond Strength 0.0621 MPa
9.00 psi
Arlon SQA-TMS-011
Arlon R37881R015 Silicone Rubber/Fiberglass
Interleave: 1.5 mil PE; Side 1: uncured silicone rubber; Substrate: 1528 fiberglass; Side 2: uncured silicone rubber; Interleave: 1.5 mil PE