Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.150 - 0.300 MPa
21.8 - 43.5 psi
on mineralic surfaces
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..
Adhesive Bond Strength 0.150 - 0.300 MPa
21.8 - 43.5 psi
on gluing mortar
BASF Styrodur® 2800 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..