Adhesive Bond Strength 0.758 MPa
110 psi
Sika Industry SikaFlex 219 LM Low Modulus Polyurethane Sealant
Sika 219 LM SikaFlex Low Modulus Polyurethane SealantThis is a high performance, low modulus polyurethane base, non-sag elastomeric sealant with excellent adhesion to a wide variety of substrates. M..