Polymer Property : Adhesive Bond Strength = 0.930 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.930 MPa
135 psi
Typical lap shear
Momentive Performance Materials RTV6702 White Adhesive Sealant, General Purpose Paste
One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose adhesive sea..
Adhesive Bond Strength 0.930 MPa
135 psi
Typical lap shear
Momentive Performance Materials RTV6703 Black Adhesive Sealant, General Purpose Paste
One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose adhesive sea..
Adhesive Bond Strength 0.930 MPa
135 psi
Typical lap shear
Momentive Performance Materials RTV6708 Translucent Adhesive Sealant, General Purpose Paste
One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: General purpose adhesive sea..