Adhesive Bond Strength 1.14 MPa
165 psi
Sika Industry SikaFlex 221 Fast Cure Polyurethane Sealant/Adhesive
Sika 221 SikaFlex Fast Cure Polyurethane Sealant/AdhesiveThis versatile product is the most popular adhesive/sealant. It is an excellent adhesive/sealant and can handle many light bonding applicatio..