Polymer Property : Adhesive Bond Strength = 1.1768 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 1.1768 MPa
170.68 psi
At 100% cohesive failure
Momentive Performance Materials RTV133 Black, Flame Retardant, One Component Silicone Sealant
RTV 133 black, one-component, ready-to-use rubber adhesive sealant is recommended for evaluation in applications in the electronic, aerospace, appliance, transportation and other industries where re..