Mechanical Properties Metric English Comments
Adhesive Bond Strength 58.6 - 86.2 MPa

@Thickness 0.508 mm
8500 - 12500 psi

@Thickness 0.0200 in
1018 steel; ASTM C633-01
The NanoSteel® Company SHS 7570 TWAS Steel Alloy, Cored Wire
Coating Description: SHS 7570 TWAS is an iron based steel alloy with a nanoscale microstructure that features exceptional combined wear, impact and corrosion resistance in high chlorine, salt fog, c..