Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.890 MPa
129 psi
Lap Shear vs. aluminum or glass
Momentive Performance Materials IGS3723 Insulating Glass Sealant
Two-component silicone which cures to form a high strength, high modulus sealant with excellent adhesion to glass. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones becam..