Adhesive Bond Strength 13.01 MPa
1887 psi
ASTM-D4541
Abatron AboCoat 8508-3 Self-Leveling Epoxy Coating and Resurfacer
AboCoat 8508-3 is a self-leveling epoxy coating and resurfacer. It is used for heavy-duty protection and rebuilding of smooth, spalled, cracked, or pitted floors. It can be applied to concrete, maso..